Sound Property Inspections
Building defects

Stepped cracks in brickwork explained

Stepped cracks follow the mortar joints of a brick wall in a staircase pattern. They can be linked to ground or footing movement, and state heritage guidance notes that buildings on parts of the Adelaide Plain may be especially prone to cracking because of clay soils. Some are minor and some point to a bigger problem. This guide explains what to look for safely, what can cause them, how serious ones differ from minor ones, and which professional should assess them.

Published 21 November 2026 · Sound Property Inspections. Drafted with AI assistance and reviewed before publication.

A stepped crack is a crack in brickwork that zig-zags up or down a wall like a staircase, following the horizontal mortar beds and the vertical joints between bricks. Many are minor, but some may point to ongoing movement in the ground or footings (the concrete or masonry base the walls sit on). State heritage guidance notes that buildings on parts of the Adelaide Plain may be especially prone to cracking because the clay soils expand and shrink with moisture. Appearance alone cannot tell you which kind of crack you have, so this guide explains what to look for, what else could be going on, and who can confirm it.[1][6][4]

What stepped cracking looks like

CSIRO's homeowner guide on footing performance describes step cracking in the mortar beds, either in the body of a wall or above and below doors and windows. It also notes vertical cracks that can pass through bricks, usually but not always in line with the vertical joints. Brickwork tends to crack at its weak points, so corners of window and door openings are a common place to find it.[1]

Measuring a brickwork crack with a crack gauge
A stepped crack following the mortar joints of face brickwork, with a clear crack width gauge card held against it.

How to check for it safely

You can learn a lot from the ground and from inside the house without climbing, opening up or disturbing anything. Look at walls from ground level and from inside rooms, and read inside and outside cracks together. South Australia's heritage guidance points out that outside cracks are often left unrepaired, so they can show a crack's history, while inside cracks may have been patched and painted over.[3]

  • Walk around the outside and note where cracks start and finish, especially at corners and above or below windows and doors.
  • Check inside the same rooms for matching cracks in plaster or at cornice corners, doors that bind, or floors that feel dished or domed.
  • Look for water sources near the walls: downpipes not connected to stormwater, leaking taps, overflowing gutters, or pooled water and soft ground after rain.
  • Note large trees close to the house.
  • Take dated photographs so any change can be compared later.

Possible causes

Bricks and mortar have very little tensile strength, meaning they cannot stretch, so some slow cracking in masonry is described as almost inevitable. When the soil under part of a wall stops supporting it evenly, the brickwork tries to bridge or overhang the gap until the bricks or mortar fail, and older masonry has little resistance to this.[4][1]

Causes of uneven support identified by CSIRO and Your Home include:[1][6]

  • Reactive clay swelling when wet and shrinking when dry, often seasonally.
  • Settlement after construction, including under poorly prepared footings.
  • Erosion or saturation of the soil from leaking water, sewer or stormwater pipes, leaking taps, faulty gutters or disconnected downpipes. Even a small leak can saturate clay.
  • Tree roots, either lifting footings or drying out the soil.
  • Poor site drainage and uneven soil moisture around the house.

This matters in Adelaide. State heritage guidance notes that buildings on parts of the Adelaide Plain may be especially prone to cracking because the clay soils expand and shrink with moisture. It also notes that trees can dry out soil under shallow footings, particularly late in a long, hot South Australian summer.[4][3]

South Australia's salt damp guide adds that some soils contain clay minerals called smectite (or montmorillonite) whose volume can change by up to 50% between wet and dry. It says these soils are commonly linked to structural cracking of masonry walls. See Reactive clay soils and cracking in Adelaide homes for more.[2]

Ground movement is not the only possible cause of stepped cracking. Other building-related causes exist, which is one reason a crack's pattern and location should be assessed by someone qualified before a cause is assumed. CSIRO also warns that because a building is stiff, movement in the soil often shows up as a rotation of the structure, so the visible cracks may not point straight at the original cause.[1]

Reactive clay swelling and shrinking (illustration)
Reactive clay swells as it gets wetter and shrinks as it dries, which can move footings unevenly.

Minor versus more serious indicators

CSIRO states that most cracking in masonry walls is a cosmetic nuisance only. Its guide grades cracks into damage categories by width, drawing on the footings standard AS 2870. Those categories come from an Australian Standard, so any assessment against them should be made by a professional using the current edition.[1]

How a crack behaves over time is often more telling than how it looks today. CSIRO explains that cracks from settlement after construction usually stop changing once settlement ends; cracks from erosion or local soil failure usually keep developing until the cause is fixed; and cracks from swelling and shrinking clay may partly stay open after each cycle and widen over repeated cycles. Many stabilise, but not always, and monitoring should be taken seriously.[1]

There is no reliable way to tell a minor crack from a serious one just by looking. Even cracks that seem to open and close with the seasons can widen over repeated wet and dry cycles, so they still need monitoring. As a practical rule, a qualified professional should assess any cracking you are unsure about. When you speak to them, mention any of the following:[1]

  • Vertical cracks through bricks. CSIRO lists these among the signs of movement, and they should be assessed along with any stepped cracking.
  • Cracked cornice corners inside, doors that bind, or floors that feel dished. CSIRO lists these among the signs of clay movement.
  • A nearby leak, a disconnected downpipe, or water ponding against the wall. CSIRO notes these can wet or erode the soil.
  • As general practice, also mention cracks that seem to be getting longer or wider, new cracks, and bricks that look displaced or out of line.
  • Cracks that seem to change with the seasons. CSIRO advises that monitoring should be taken seriously, so ask the professional whether and how these should be monitored.

In a double-brick house, CSIRO advises that internal cracking deserves the most attention, with external cracks a useful guide to stress on the structure. In a brick veneer house (a timber or steel frame with a single outer brick skin), the frame behaves differently, but the outer brick skin cracks much like a double-brick wall. For broader guidance, see Cracks in brick walls: when to worry.[1]

What happens if it's ignored

Where the cause is ongoing, such as a leaking pipe eroding the soil, cracking usually continues until the cause is dealt with. Reactive clay movement can also cause cracks to widen with each wet and dry cycle. Your Home notes that cracks and settlement can be cosmetic or a sign of more serious structural problems, which is why the cause matters more than the crack itself.[1][6]

Is professional investigation needed?

In most cases, yes, because the cause and seriousness of cracking can't be judged from appearance. Your Home recommends getting expert advice for cracks and settlement. South Australia's salt damp guide says that where reactive clay is causing structural cracking, advice should be sought from a geotechnical engineer (a specialist in soils and foundations). Only investigation can confirm whether reactive clay is the cause. As a general rule, a pre-purchase building inspection is a visual inspection. It can record where cracking is and recommend further specialist assessment, but it should not be relied on to confirm a cause. See What's included in a pre-purchase building inspection in SA. If an inspector or engineer suggests monitoring, they can advise how and for how long.[6][2]

For context, the National Construction Code (NCC 2022 Housing Provisions, Part 4.2) explains site classes for footing design, from Class A (sand and rock, little movement) through Classes S, M, H and E (increasingly reactive clay) to Class P (problem sites such as soft or collapsing soils or abnormal moisture). South Australia also has its own engineering provisions for residential footing design. These are design documents for engineers; check the current edition applying in South Australia before relying on them.[5][7]

Common repair approaches

Repairs should be based on the confirmed cause. As general good practice, that means finding and fixing the cause first, monitoring any movement, and only then repairing the brickwork. CSIRO describes footing repair as generally specialist work and says any excavation near footings should be properly engineered. Typical approaches, depending on the cause and professional advice, include:[1]

  • Fixing leaking pipes, taps and gutters, and connecting downpipes to stormwater.
  • Improving surface drainage so water flows away from the walls.
  • Managing trees and garden beds close to the house, on professional advice.
  • Repairing cracked brickwork and mortar once movement is understood.
  • Any footing repair, which CSIRO describes as specialist work, carried out only on an engineer's advice.

Older homes also raise a balancing act. The salt damp guide notes a trade-off between keeping soil moist to limit cracking and drying walls to limit rising damp, so engineering advice on cracking should also consider any damp treatment.[3][2]

Who to call

  • Building inspector: to look at the cracking in the context of the whole house before you buy.
  • Geotechnical engineer or specialist consultant: South Australia's salt damp guide says a geotechnical engineer should be consulted where reactive clay is causing structural cracking, and CSIRO describes footing repair as specialist work.
  • Structural engineer: as general practice, where cracking may be structural, a structural engineer should be asked to assess it and design any structural repair.
  • Plumber: to find and repair leaking water, sewer or stormwater pipes and connect downpipes.
  • Bricklayer: as general practice, brickwork repairs and repointing should wait until the cause has been addressed and should be done by a bricklayer or masonry tradesperson. For lime-mortar walls, choose one experienced with older masonry.

Prevention

Most prevention is about keeping soil moisture around the house even. CSIRO recommends fixing plumbing faults, connecting downpipes, adding surface drainage, and laying a paved apron around the house, which it suggests be at least 900 mm wide with a fall of 1:60. South Australian heritage guidance similarly suggests checking for pooled water or soft ground within 4 m of the walls after heavy rain.[1][3]

Stormwater ponding against a brick veneer wall
Stormwater ponding beside a brick wall after rain, a condition that can wet the soil next to the footings.

Related pages

Are stepped cracks in brickwork always structural?

No. Most masonry cracking is cosmetic, but stepped cracks can also signal ongoing ground or footing movement. Whether they are serious depends on the cause, width and whether they are changing, which a qualified professional should assess.

Why can Adelaide homes be prone to stepped cracking?

Parts of the Adelaide Plain have clay soils that swell when wet and shrink when dry, which can move footings unevenly. Leaks, poor drainage and nearby trees can make this worse.

Should I just fill the crack?

Not before the cause is understood. Filling a seasonal crack at its widest can push the wall out of line, and cement mortar is unsuitable for older lime-mortar walls.

Who should assess stepped cracking before I buy?

A pre-purchase building inspection can identify and record the cracking. Where it looks significant or active, a geotechnical or structural engineer should investigate the cause.

If you're buying a brick home with stepped cracking, a [pre-purchase building inspection](/pre-purchase-building-inspection-adelaide) can help you understand what you're looking at before you commit.

Book Inspection

This page is general information about what a condition may indicate. It is not a diagnosis of any particular property: only an inspection, and where needed a specialist, can confirm a defect and its cause.

Sources

  1. Foundation Maintenance and Footing Performance (Building Technology Resource) — CSIRO. Accessed 2026-11-18.
  2. Salt Attack and Rising Damp (technical guide) — Government of South Australia, Department for Environment and Water. Accessed 2026-11-18.
  3. Maintenance and Repair of Older Buildings in South Australia (Heritage Technical Note 3.1) — Government of South Australia, Department for Environment and Water. Accessed 2026-11-18.
  4. Early Bricks and Brickwork in South Australia (Heritage Note 3.3) — Government of South Australia, Department for Environment and Water. Accessed 2026-11-18.
  5. NCC 2022 Housing Provisions, Part 4.2 Footings, slabs and associated elements — Australian Building Codes Board. Accessed 2026-11-18.
  6. Repairs and maintenance — Your Home (Australian Government). Accessed 2026-11-18.
  7. Special Provisions for the design of residential slabs and footings, South Australian conditions (April 2026) — Engineers Australia. Accessed 2026-11-18.

Related

Book Inspection